Analysis of Interface Fracture of Cold-Sprayed Coatings Due to Thermal Cycling
Journal of Thermal Spray Technology, ISSN: 1544-1016, Vol: 29, Issue: 1-2, Page: 158-172
2020
- 4Citations
- 12Captures
Metric Options: Counts1 Year3 YearSelecting the 1-year or 3-year option will change the metrics count to percentiles, illustrating how an article or review compares to other articles or reviews within the selected time period in the same journal. Selecting the 1-year option compares the metrics against other articles/reviews that were also published in the same calendar year. Selecting the 3-year option compares the metrics against other articles/reviews that were also published in the same calendar year plus the two years prior.
Example: if you select the 1-year option for an article published in 2019 and a metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019. If you select the 3-year option for the same article published in 2019 and the metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019, 2018 and 2017.
Citation Benchmarking is provided by Scopus and SciVal and is different from the metrics context provided by PlumX Metrics.
Example: if you select the 1-year option for an article published in 2019 and a metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019. If you select the 3-year option for the same article published in 2019 and the metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019, 2018 and 2017.
Citation Benchmarking is provided by Scopus and SciVal and is different from the metrics context provided by PlumX Metrics.
Article Description
Driving mechanisms for the interface delamination of cold-sprayed chromium on a steel substrate subjected to cyclic thermal loading are studied by using thermomechanical analysis. First, the equilibrium stress states of the coating system due to residual stresses are determined for different coating thickness vales. This system is then subjected to periodic heating and cooling cycles. The potential of crack initiation and growth is simulated with and without embedded micro-cracks. The corresponding crack-driving forces are characterized using the interface stresses and energy release rate as a function of the thermal cycles. The effects of coating thickness, location of the embedded micro-cracks and initial residual stress on these driving forces are investigated systematically to demonstrate the risk of coating fracture and delamination.