PlumX Metrics
Embed PlumX Metrics

Influence of lattice stability on hydrothermal deactivation of Cu-ZSM-5 and Cu-IM-5 zeolites for selective catalytic reduction of NO x by NH 3

Journal of Catalysis, ISSN: 0021-9517, Vol: 309, Page: 477-490
2014
  • 130
    Citations
  • 0
    Usage
  • 94
    Captures
  • 0
    Mentions
  • 0
    Social Media
Metric Options:   Counts1 Year3 Year

Metrics Details

  • Citations
    130
    • Citation Indexes
      129
    • Patent Family Citations
      1
      • 1
  • Captures
    94

Article Description

Copper-exchanged zeolites are well-known catalysts for the selective catalytic reduction of nitrogen oxides by ammonia (NH 3 -SCR). To determine the influence of framework stability on catalyst deactivation, two zeolite frameworks, MFI and IMF, were used in this study. The two frameworks have similar window size and connectivities, but the IMF structure is less susceptible towards dealumination. In each zeolite, copper was introduced by aqueous exchange and the catalytic performance in the NH 3 -SCR reaction compared before and after hydrothermal ageing at 650 and 750 °C. The changes in state and local environment of Cu and the degradation of the zeolite structure were characterized using ammonia capacity measurements, solid state nuclear magnetic resonance, X-ray fine structure spectroscopy, temperature programmed reduction with hydrogen, infrared spectroscopy monitoring of adsorbed NO and CO probe molecules as well as the combination of transmission electron microscopy and energy dispersive X-ray spectroscopy to follow copper migration. The catalytic performance of Cu-ZSM-5 and Cu-IM-5 is similar in the fresh state, but after hydrothermal ageing the deactivation of Cu-IM-5 is less severe compared to Cu-ZSM-5 as a consequence of the higher framework stability. The changes in catalyst structure that occur during ageing are (i) partial dealumination of the zeolite, (ii) reversible migration of copper species, and (iii) irreversible formation of catalytically inactive and stable Cu–Al clusters, which have some resemblance to CuAl 2 O 4, but without the symmetry of Cu in the spinel structure. As the Cu–Al clusters only form once Al is detached from the framework, the stability of Al in the zeolite framework is proposed to dictate the overall hydrothermal deactivation behaviour of Cu-ZSM-5 and Cu-IM-5 in the NH 3 -SCR reaction.

Bibliographic Details

Peter N.R. Vennestrøm; Ton V.W. Janssens; Arkady Kustov; Marie Grill; Anna Puig-Molina; Lars F. Lundegaard; Ramchandra R. Tiruvalam; Patricia Concepción; Avelino Corma