PlumX Metrics
Embed PlumX Metrics

Achieving porous tungsten with high porosity by selective dissolution of W-Fe alloy

Scripta Materialia, ISSN: 1359-6462, Vol: 198, Page: 113830
2021
  • 17
    Citations
  • 0
    Usage
  • 10
    Captures
  • 0
    Mentions
  • 2
    Social Media
Metric Options:   Counts1 Year3 Year

Metrics Details

  • Citations
    17
  • Captures
    10
  • Social Media
    2
    • Shares, Likes & Comments
      2
      • Facebook
        2

Article Description

Porous W with high porosity of 75.7 % was achieved by selective dissolution using Fe as active elements. The results showed that W-Fe pseudo alloy precursor was sintered at 800°C, the nano C powder helped in-situ formation of the W 6 Fe 6 C phase and the interface of W-W and W-Fe were both combined by W 6 Fe 6 C. It enabled the precursor to inherit the morphology of the green compacts without deformation. W-W connection remained and formed W framework after the selective dissolution of Fe. With the increasing of heat treatment temperature, the porosity decreased and the compressive strength increased, the change of the pore size is very little due to the effect of the W 6 Fe 6 C in the W framework.

Provide Feedback

Have ideas for a new metric? Would you like to see something else here?Let us know