Room-temperature hard coating of ultrananocrystalline diamond/nonhydrogenated amorphous carbon composite films on tungsten carbide by coaxial arc plasma deposition
Japanese Journal of Applied Physics, ISSN: 1347-4065, Vol: 55, Issue: 3
2016
- 14Citations
- 2Captures
Metric Options: Counts1 Year3 YearSelecting the 1-year or 3-year option will change the metrics count to percentiles, illustrating how an article or review compares to other articles or reviews within the selected time period in the same journal. Selecting the 1-year option compares the metrics against other articles/reviews that were also published in the same calendar year. Selecting the 3-year option compares the metrics against other articles/reviews that were also published in the same calendar year plus the two years prior.
Example: if you select the 1-year option for an article published in 2019 and a metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019. If you select the 3-year option for the same article published in 2019 and the metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019, 2018 and 2017.
Citation Benchmarking is provided by Scopus and SciVal and is different from the metrics context provided by PlumX Metrics.
Example: if you select the 1-year option for an article published in 2019 and a metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019. If you select the 3-year option for the same article published in 2019 and the metric category shows 90%, that means that the article or review is performing better than 90% of the other articles/reviews published in that journal in 2019, 2018 and 2017.
Citation Benchmarking is provided by Scopus and SciVal and is different from the metrics context provided by PlumX Metrics.
Article Description
Ultrananocrystalline diamond (UNCD)/nonhydrogenated amorphous carbon (a-C) composite films were deposited on unheated WC containing Co by coaxial arc plasma deposition. The hardness of the film is 51.3 GPa, which is comparable with the highest values of hard a-C films deposited on nonbiased substrates. The deposited film is approximately 3 ?m thick, which is one order larger than that of hard a-C films. The internal compressive stress is 4.5 GPa, which is evidently smaller than that of comparably hard a-C films. The existence of a large number of grain boundaries in the UNCD/a-C film might play a role in the release of the internal stress.
Bibliographic Details
http://www.scopus.com/inward/record.url?partnerID=HzOxMe3b&scp=84962032616&origin=inward; http://dx.doi.org/10.7567/jjap.55.030302; https://iopscience.iop.org/article/10.7567/JJAP.55.030302; http://stacks.iop.org/1347-4065/55/i=3/a=030302?key=crossref.1ed5f650a88c4ce2c0206dc93ed075e2; http://stacks.iop.org/1347-4065/55/i=3/a=030302/pdf; https://dx.doi.org/10.7567/jjap.55.030302; https://validate.perfdrive.com/fb803c746e9148689b3984a31fccd902/?ssa=776ba7d1-2847-4c2f-b0e0-223c69f485ca&ssb=69230266485&ssc=https%3A%2F%2Fiopscience.iop.org%2Farticle%2F10.7567%2FJJAP.55.030302&ssi=c2d038b9-8427-49d0-96f7-e01a1d8e8e30&ssk=support@shieldsquare.com&ssm=12768223874720645987736999934286379&ssn=0f9d74474e28d760c288a7d31595e0a65c70e7e44089-5b4c-4bba-92f5e5&sso=4527980e-62ddb6055d96d20ee66f47aa9b5c5625aaf08d5461337553&ssp=70694622591722194886172234750444504&ssq=61388018704749783813796580047845536871033&ssr=NTIuMy4yMTcuMjU0&sst=com.plumanalytics&ssu=&ssv=&ssw=&ssx=eyJfX3V6bWYiOiI3ZjYwMDA3NmNmYmIwZC1hOTY5LTQwMjItYWM3My04NjU0NDg0NTczMTgxNzIyMTk2NTgwNDk0MTkwNDY2NTMwLTczNGRjNzBiNzdjYWVlNmI5ODc2MSIsInV6bXgiOiI3ZjkwMDA1ZmViNjE3Ny05MmVkLTRmNTYtOGZlMS01OTlkOWM5MmM0MTU0LTE3MjIxOTY1ODA0OTQxOTA0NjY1MzAtYzc1ZDRlZGYwZjM0NmQyZjk4NzUyIiwicmQiOiJpb3Aub3JnIn0=
IOP Publishing
Provide Feedback
Have ideas for a new metric? Would you like to see something else here?Let us know